Just done a quick test.. what do you guys think?

http://www.talkcomposites.com/Topic19916.aspx

By morepower - 12/2/2015 12:50:30 AM

Been testing a new material which is still a development formulation. I had to make some air box parts for a customer but I got to make a velocity stack from the stuff to test and its very good.. Just out of the mould with no lacquer it has stunning clarity. I only had scraps to use for the velocity stacks so this is made with those scraps.


Yes there is a small blemish on one bit (my fault) but no other pinholes at all... 
By morepower - 12/25/2015 8:35:03 PM

I know the guy used ATLAC 580 tooling and I think it is a Nord Composites vinylester gelcoat.