By deagrateful - 11/10/2015 2:25:48 PM

Over a year ago I attended Easy Composites 3 day training course as I had a new piece (I'm a furniture designer) that was to be made entirely of carbon fibre. Anyway, long story short the chair is finished and has been very well received by the design world. I would just like to say thanks to Paul, Matt and Warren (and several forum members) who solved many problems along the way. I would be happy to answer any questions about the build if there's interest. Full pics can be found on my website krislamba.com

http://payload397.cargocollective.com/1/13/420588/10252260/Rv1-factory-2_1000.jpg
http://payload397.cargocollective.com/1/13/420588/10252260/front-view-4_1000.jpg
By VVS - 11/17/2015 1:09:32 PM

Yes very impressive and interesting design. Smile