By clyons - 10/14/2015 5:20:23 PM
Hi I am creating a carbonfiber body for a small prototype car, I was thinking of embedding timber mounting brackets into the body, I was just wondering if this was possible and how best to go about doing it.
Thanks
|
By Dravis - 10/16/2015 12:37:44 PM
Then I would use infusion, with a peelply backing, and then laminate in the wood afterwards... Alternatively seal the wood with epoxy when cut/sanded to shape, wrap them in peel-ply - then cure
When laying up the "stack" for infusion remove the peel-ply from the wood inserts, then just add them inside the infusion "stack" (I do this with roughly sanded metal inserts)
|
|