Talk Composites - The Forum for Advanced Composites

Shade Cloth as an infusion mesh

http://www.talkcomposites.com/Topic19503.aspx

By Frobisher - 10/11/2015 12:54:22 AM

I've heard of hardware store shade cloth being used as a cheaper alternative to infusion mesh.

Has anyone here tried it? Was it successful?
By Frobisher - 10/12/2015 2:42:26 PM

That's less encouraging. I'm going to do some test runs so I'll try the shade cloth and see how it turns out.