By twissta - 1/23/2012 4:58:43 AM
Hey Fam,
The PDF file that gives you the directions for the Uni-MOLD system requires 150g of (CSM) with the coupling coat, followed by 450g 0f (CSM) of the tooling resin?...............
I want to use cabon fiber so would insert the correct size weight of (FRP) in place of the (CSM)....?
to complete the Part...or
Is this the foundation or completed tooling for the mold to begin laying carbon fiber laminates parts......
|
By batbyggare - 3/5/2012 8:28:50 PM
this whas my first mould with a similar uni-moulding system.http://www.ribunlimited.se/rib.html
It whas realy nice to work with.
Its a 36 fots RIB and i make all the moulds with uni-mould..
All the pluggs was cnc milled and the constuctor was Egil Ranvig from Norway, he was the owner of Hydrolift.
|
|