Hello

What is the ideal ambient temprature for applying: 

- Epoxy tooling gelcoat and epoxy mould putty?
- Uni mould gelcoat, coupling coat and tooling resin?
By Dravis - 10/1/2015 11:15:47 AM

19 - 21  degrees Celcius, not too high humidity ...