Carbon pacifier (dummy teat)
http://www.talkcomposites.com/Topic19190.aspx
By Brucecreations
-
9/13/2015 3:43:48 PM
A special gift for a friend who became a father of two beautiful twins
It was a funny experience.
In these cases, decorative fabrics are very useful
More photo here
https://plus.google.com/+Brucecreations77/posts/AAT2mvjTRaX
By Brucecreations
-
9/14/2015 7:51:22 AM
Is it solid carbon or is it a plastic dummy wrapped in carbon?
Thank you, they are full carbon, I used the plastic one like a core in the mould of the handle.