Talk Composites - The Forum for Advanced Composites

Newbie from France

http://www.talkcomposites.com/Topic18993.aspx

By macsddau1 - 8/10/2015 5:14:51 PM

Hi,

I'm new to composite. I have the basic knowledge learned at the CETIM (http://www.cetim.fr/en). For hobby, my interest cover pattern, mould making and resin infusion.
For pattern, I print shapes on a 3D printer using PLA (I tried with foam has EC method, but I don't have a gift for this), glue them, and then start with EC pattern coat primer...
For the moment I have make 2 moulds but second have leakage. I will post in other topic about this.
In the first mould, I make 2 times a composite part but I'm not satisfied of the result. In sharp corners the fabric don't stick the the shape an there are a lot of bubbles.

I hope to improve my work with the community.
By matthieutje65 - 8/14/2015 10:26:21 PM

Salut denis, 

t'as de la chance d'avoir un voisin Belge Ici Wink
To keep it simple I do think it will be easier to keep everything in English