By Ronny - 8/10/2015 11:47:05 AM
Hi Im new to this and tried skinning a fuse cover.
I did the following rough sanding with 400 grit Rinse with industrial cleaner and lighter fluid One layer with EC epoxy base coat Then i waited approx 2hours when it was tacky with no paint coming off. Then i applied one 200g 2twill pro finish layer, cut it formed it and put masking tape around the edges of the carbon. A thick layer of laminating resin was applied. After this i covered all the carbon area with peel ply and on top of that a layer of breather cloth and the bag connector. Then sealed it all with plastic and managed to get a leak free seal. Let it stay over the night and removed the peel ply.
what i found was that the carbon was firmly in plase, but there was alot of print through and the carbon looks almost dry.
So when using this technique do i have to put on additional layers of resin and vacuum bag it again and again? How do i reduce the peel ply print on the carbon?
|
By matthieutje65 - 8/16/2015 6:46:40 PM
thanks ronny
|
|