Ok, i think im going to have to de mould first but it's not an important part really, just a cover.
Can you recommend a good ramp rate? Is 1 degree a min slow enough?
Also does the post cure have to be done in one cycle?
10hrs at 60 degree one day, the next day 2hrs at 70 degrees and so on.
Bit worried about leaving my oven one all that time