7/24/2015 5:58:25 PM
I was going to use the EC uni mould system but i don't like the face it can only go up to 80 degrees c.
Which means 10 hours to cure the pre preg. (correct me if I'm wrong)
Would like lowest cure time possibly.
Are there any other options in high temp mould materials?
By Darren
-
7/25/2015 5:55:52 PM
Ok i shall stick with uni mould.
Good to hear it can go up to 100 degrees.