By twissta - 7/23/2015 12:04:10 AM

Is it ok to put parts into use if you let it cure at room temperature? What are the end problems or results with this process? The parts will be exposed to the elements, because they are motorcycle part for cosmetic appeal.

Thanks in advance,  guys!
By ArturK - 6/14/2016 9:46:41 AM

Without post-curing you will notice "print" at carbon fiber after exposing to sun.
Many epoxy resin are a little bit brittle without post-curing.

I always advice to post-cure carbon fiber parts even to 50-60 C .