Talk Composites - The Forum for Advanced Composites

Wanna Thank you Easy composites

http://www.talkcomposites.com/Topic16841.aspx

By TomDesign - 5/3/2015 6:24:08 PM

Wanna Thank you guys for your product-Fillet wax.

I work 8 years with composites- But never had thing like this. So easy to work!!Amazing!
By Matt (Staff) - 6/6/2015 11:01:40 AM

Hi Tom,

Thanks for the comment. Yes, it's a really fantastic material. Like most people, we 'grew up' using plasticine for filleting, filling and temporary barriers but, as you say, the yellow wax is a world apart in terms of how easy it is to shape and smooth.