Talk Composites - The Forum for Advanced Composites

resin table top

http://www.talkcomposites.com/Topic16758.aspx

By willrenner - 4/27/2015 1:59:12 PM

Sorry if this is covered elsewhere, I couldn't find it.

I have made a table with parquet floor tiles laid onto plywood, and would like to shutter the edges and pour some kind of epoxy on to make it completely smooth. What would be the best product? and are there any pitfalls I should be aware of?

Many Thanks

Will
By leerobo - 6/3/2015 5:09:07 PM

I was wondering if you progressed any further on this subject as ive spent hours looking for a clear resin that can handle a under floor heated penny floor ?