By batbyggare - 5/14/2012 8:59:16 PM
I while ago i asked aboute polyester moulds and epoxy infusion...
U answerd me to try with pva, it would woork if the moluds is old.
Now ihave tryed one time with pva and one time with easy-lease and it dosent woork so good.
I wonder if i can spray my moulds with pu carpaint?
Best reugards Magnus
|
By batbyggare - 5/15/2012 12:36:25 PM
I have some trouble with demolding..small parts of epoxy stick to the mold..
Matt explained that the polyester let go of the solvent for a long and the epoxy does not like where to stick it a little in molds.But are the molds old i can work werry well. So my idea is to spray pu varnish to seal off the polyester.
|
|