Hi all Have recently started dabbling in carbon composites and have been massively impressed with the help from the guys at easy composites!!
Am still buzzing off the back of carbon success, but am expecting to encounter the messy side very soon.
Iv got a large project on at the minute and am currently seeking advice on the best way to join a carbon beam to the top of a carbon boat hull, best idea at present is to epoxy the tube to the top of the hull and then reinforce with small carbon wraps!
Any better suggestions would be greatly appreciated!!