By gordon55 - 4/17/2015 12:55:58 PM
Hello -- is it possible to colour your Coating Resin? I would like to give it a colour (preferably white) as it's easier to see contours for sanding than if it's clear.
Many thanks, GW
|
By Jacopo Carbonio - 4/20/2015 9:50:17 AM
I tried red pigment for resin and if you want to make the resin become completely red with no refrection you have to use more pigment..but great result I used red one and it was perfect
|
|