i want to know is there any advantage of using intermediate modulus fiber having 440 tex inspite of standard modulus 880 tex?how the weight will be saved? because thickness buildup by 440 tex will be half of 880 tex (i think so).and in the end both material will give same weight of product.
can any one explain how weight saving is achieved in using intermediate modulus fibers?