By SlinkyDGE - 3/18/2015 12:28:41 PM
Hi,
I understand from various sources that I need to pre-coat paper and photos before imbeding them in epoxy/resin. I can't exactly find the product I need to use and wondered if a simple clear acrylic spray would work and keep the image safe and colourful?
Thanks for your advice.
Linda.
|
By Warren (Staff) - 3/19/2015 10:00:56 AM
An even coating of PVA wood glue will seal the paper from the resin thus preventing the paper being ruined.
|
|