Hello everyone
This is my first post but I have read on the forum for a year
Okay my question
I will make a roof for a bmw e90 is about 1.5 square meters
I made the mistake and ordered fast hardener do you think it will work?
Will it work with one resin inline or will I need more inlines?
If I need more lines how will I lie it down?