Talk Composites - The Forum for Advanced Composites

After waiting for the gel coat to get into its squeaky state

http://www.talkcomposites.com/Topic155.aspx

By Daz - 1/21/2012 11:08:38 PM

,how long do you wait for the coupling coat

If at all ,

Do you go straight ahead with the tooling gel or do you have to wait for the coupling coat to go of like the gel coat 

before laminating the  rest of  the mold ,

Can u tell im new to this lol
By Daz - 1/23/2012 6:28:31 PM

Cheers again Paul,