By mhrluscombe - 5/4/2012 12:26:59 PM

Hi,

I'd like to construct an exhaust box from carbon fibre, around 40cm x 30cm x 20cm. The exhaust gases are around 600'C. What is the temperature capabilities of carbon fibre sheet & edging, and is there a high temperature means of bonding to construct a box from these materials?

Cheers, Mark.

By Matt (Staff) - 6/26/2012 1:41:00 PM

Hi Mike,

Exhaust tips are perfectly feasable, they're well within the temperature of our high temp epoxy.