Talk Composites - The Forum for Advanced Composites

hand carbon fiber work

http://www.talkcomposites.com/Topic15104.aspx

By elsitioNet - 2/17/2015 7:04:14 PM

Hi 
few questions about material's  
I don't  have infusion  tools and I want to make this fenders flares in Carbon Fiber.
but first I have to make a mould.. the last picture is an example of the part 
I don't have idea of the fiberglass and CF size and weight for small project like this..
the resins are the same for infusion and hand work?
after that I want to do some parts for my car with black CF and red Kevlar
I saw all your videos I have some old school experience in Fiberglass 20 years ago
then my car is an other project