Hi all I have just started my first bonnet mould using the unimould system only it hasnt gone to plan.
the mould has came out with fine cracks through the middle and it broke in places where it locked on
My question is could i spray a gelcoat of some kind into the mould and give it a fresh layer because the cracks look to much to fillor maybe another way somebody could suggest