By JCCR - 1/31/2015 10:51:53 PM				
            
                      
            Has anybody tried making a mould out of nylon or some other kind of easily machinable material? I am going to make an aluminum mould for the final part but would like to try out some kind of quick mould first before investing the time in machining the aluminum. I know the surface finish won't be as good though. Thanks
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 2/2/2015 2:17:04 PM				
            
                      
            Our Mouldphorm PCL Low-Melt Thermoplastic is a good temporary mould material.  Dead easy to use and epoxy, PU,  polyester and vinylester don't stick to it so no need for release agents.
           
		 | 			
		 
	
	
						
		 	
		
	 |