Hi everyone
When i first started up i brought a roll of mti and allthough it works well i just cant see it being cost effective being how much it is and how much u have to use 

I was wondering if i could use it the same as matt in the ec vid and just use a strip along the outlet like u would with the spiral tubing 
My thinking is surley the logic is the same and it will pull the resin to it and not let it thru whilst still pullin the air out the part

its just an idea as i have about 10m kick8b about with no use for it nemore 
 Thanks daz
By prsw - 12/19/2016 9:28:53 PM

which video are you talking about?