I want to make a concrete sculpture for an art project I am working on. After doing some research I am under the impression that I could use MDF as a cast as long as I coat it with a suitable release agent. Can Easy-Lease be used to coat MDF for a cast which will hold concrete?
By ChrisR
-
1/26/2015 2:28:00 PM
How big / shape etc are you trying to make? Is it a single use mould? etc
Find a local building site (larger development rather than small builder type) and ask them for some shuttering release oil.