By Racing_34 - 1/18/2015 7:15:13 PM
hi guys, i've bought a resin infusion starter kit, i followed the video tutorial but i'm failing to obtain the desired vacuum level. I can clearly hear a leak from the vents, i've tried several times to do the bagging from scartch, to use more gum tape around the tube, to put gut tape both inside and outside the bag, but still i've a huge leak, the gauge doesn't go under -0.5 bar. how can i improve vent sealing?thank you!
|
By Racing_34 - 1/22/2015 10:32:03 PM
hi guys thank you for your answers, tried it over and over and now i'm having good results  cheers
|
|