By cpalada - 1/14/2015 9:39:16 AM

Hi everyone,

Long time lurker here. Have been following these forums for a while and have been slowly learning lots of things from everyone. 

I have all of the equipment for vacuum infusion and decided to take the plunge and have a go. For my first project i'm keeping it small - my car has these terrible looking plastic trim bits that are hydro-dipped with a carbon fibre pattern. so naturally I want to make them of real carbon fibre!

The shape is very simple (I think makes a great first project), the only problem I'm having is coming up with a way to make the mounting tabs on the back of the piece. see photo links down below

By FLD - 1/15/2015 2:43:38 PM

What he said!