By pinheirofox - 1/12/2015 9:05:18 PM

good night!!I have a question about epoxy resin. for 1 m2 of carbonfiber how much i need resin?!


thanks
By ajb100 - 1/12/2015 10:49:25 PM

The above link is good.

General rule of thumb is  50% fibre weight, 50% resin. So 1m2 of 200gsm needs 200g of resin......generaly