By boustie - 4/29/2012 8:29:09 PM

Turned out ok ish for my first attempt but i have a slight issue where small areas of the resin have stuck to the steel mould i have.

Any ideas why this may be / pointers ?. Third picture shows the steel mould where the epoxy has stuck slightly.

I used 4 layers of carbon, wet lay with peel ply, release film, fabric and then vacuum bagged it

Thanks, Pete.

http://i230.photobucket.com/albums/ee247/boustie/IMAG15662.jpg
http://i230.photobucket.com/albums/ee247/boustie/IMAG1564.jpg
http://i230.photobucket.com/albums/ee247/boustie/IMAG1565.jpg
By boustie - 4/30/2012 5:21:55 PM

how many layers of carbon should i typically use, size is approx 12cm x 60cm. Part use as and engine cover