My bonnet is Down to bare metal, do I have to paint it or can I just use epoxy resin, then flat and polish,
before making a mold?
Best Regards Tortit
|
By ajb100 - 12/31/2014 9:27:50 PM
If the metal is smooth then it's fine. Prefer working from bare metal as there's never the worry of paint damage
|
|