By neilb - 4/27/2012 10:58:45 AM
can i use a filled epoxy resin as a gelcoat?
the uni mould system from ec would be ideal but at the moment it cannot be shipped to oz
|
By Joe - 4/27/2012 3:11:10 PM
Hi,
I cant answer this question, but I had about the same question here.
Hopefully the other guys will have more precise answers.
|
|