Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Equipment and Materials
best place for vac gauge
http://www.talkcomposites.com/Topic1423.aspx
By boustie
-
4/26/2012 9:56:30 PM
Where is the best place for a vac gauge when wet laying in a vac bag.
By Joe
-
4/27/2012 2:32:28 PM
Hi,
The most far you can from the vacuum line.