Hiya
Well this aint easy is it
hoping for loads of help
just a quickie, why dus the epoxy resin go cloudy ????
ta
owen
By spec-naz
-
11/19/2014 12:26:48 PM
It's not a bag. It is mould side, so it was touching just wax and release agent PVA. But after post curring this side effect disapeared