matthieutje65 (15/11/2014)
Hanaldo (15/11/2014)
Wasn't a miscalculation, I was just using a 60/40 fibre/resin ratio which is what I normally aim for with infusion. You won't get that with wet lay unless you are very good. oh ok hanaldo you were talking about 265/sqm

thought for the full 2sqm

Haha no no, 265 grams for the full 2 meters. With a 60/40 ratio, 1sqm of 200g carbon cloth will use 133 grams of resin