hello. My name jehyun
I'm clumsy English.
Why did this happen?
The pinholes
how to: Resin infusion
By Dravis
-
11/12/2014 10:59:29 AM
Low on Resin, leaky bag ?? No infusion mesh / mesh not covering entire piece ?