after a lot of trial and error... and a lot of help and guidance from the boys.... I've finally made something for my hillclimb car that I can share...
most of the parts I have already made were made for lightness and as such... aren't that pretty, but there damn light
Still to be trimmed to shape and cleaned up with another to be made. This one is fresh out of the bag...
4 layers of 200gsm CF & vac bagged
By tangotop
-
4/24/2012 6:12:23 PM
Cheers Matt
forgot to say that this was cured off at 60deg...