Talk Composites - The Forum for Advanced Composites

Historic Porsche Parts

http://www.talkcomposites.com/Topic13546.aspx

By TWINFOX - 11/2/2014 3:38:57 PM

Hello from Germany

I'm joining this forum since some time and now I have decided to show some of my works.
I make engine covering parts for historic Porsche racecars.
The pictures shows a 910 engine with the parts I've made.
All parts are wet layer in multi-part moulds, with epoxy.

http://www.talkcomposites.com/Uploads/Images/3a391c09-9920-412a-b99d-db9d.JPG


http://www.talkcomposites.com/Uploads/Images/c7001aa0-e9a7-41c4-ae7f-3592.JPG


http://www.talkcomposites.com/Uploads/Images/6c7b73db-623d-4e61-aaf9-4176.JPG




http://www.talkcomposites.com/Uploads/Images/66eeac4a-22eb-4aa8-9d81-52c0.JPG
By TWINFOX - 11/10/2014 6:52:13 PM

Bonobo (04/11/2014)
Very Nice!

Are these reproductions of original vintage parts?


Thanks Smile
Yes, theese are reproductions, but with higher quality epoxy resin.