By JaWillis - 10/25/2014 2:45:36 PM

Any advice on how to adhere your prefab carbon tubing to pre-preg carbon fiber? Example: a 42mm ID tubing which happens to be the exact size id of a bicycle Bottom Bracket PF30. (press fit 30). However I need to beef up the wall thickness (add 1/16 ") by wrapping pre-preg around it, then compress and heat to cure. I am concerned there may be a delamination issue between the tubing and the pre-preg. Is there something I need to treat the tubing with prior to applying pre-preg? 

Thanks in advance for your help.
By JaWillis - 10/26/2014 11:02:58 AM

Good to hear. Thanks!!