Do I need to put a wax additive in the Uni-mold gel coat to use it to repair some damaged in a mold.
By Warren (Staff) - 10/20/2014 11:33:59 AM

You can use a wax additive. Use some fresh gelcoat mixed with a little Solution MW Wax Gelcoat Additive to prevent the cured resin being tacky. Then once cured, sand flat with surrounding gel and polish back up.