As a hobby I make FRP/glass fibre parts for MGBs and TR7/8s - morSpeed Performance Products. I use polyester resins and gel coats in poly molds that have poly tooling gel coat surfaces.
I'm starting into vacuum forming to make the parts thinner, stronger, and with less resin. However, I'd like to start using epoxy (then, into infusion) for some of my parts.