By heiwaz - 9/13/2014 9:38:26 PM

Hello, I want to try skinning car parts with prepeg carbon, but i have seen that there are different types of prepegs, with resin in one side and resin on both sides. What is the better choice for skinning?
By ChrisR - 9/19/2014 10:44:55 AM

When working with compound curves, I've always found it easier to wet out a normal dry fabric off the part (creating my own pseudo prepreg) then laying it up onto the mould. The other way I've done it is to lightly spray tack the fabric to gently hold the pattern while handling.