Hey all,
Having recently started my own composites business, I found myself doing a large amount of work for a local workshop/race support team here that deal with all-out track cars (and people with entirely too much money). The workshop have got so much work for me to do that I don't really have time to do anything else at the moment, but over the last month or so my main project has been the Lotus Exige that they have.
Long term, the customer wants to build the entire thing barring the chassis from carbon fibre. Fortunately my job is made easier given the car is basically a block of aluminium for a chassis and the rest is fibreglass bolted on, so everything is designed to work with composites. The first part I made for them was a simple dash mount for the Motec C185 digital dash, which I had to design and build from scratch: