By biker_kev - 8/21/2014 1:23:17 PM
Hello,
I want to apply a carbon fibre skin to some motorcycle exhaust end caps. The existing end caps are already made of carbon fibre, but they have become damaged. I was planning to repair the mouldings from inside using high temperature resin, then skin the outside. Due to the cost I was considering using the clear high temperature resin and mixing in some black pigment to apply as a basecoat rather than buy the separate black basecoat resin. Is there any reason why this would not work?
Kevin
|
By biker_kev - 8/22/2014 5:24:21 PM
Thanks for the info.
Kev
|
|