Infusion Problem...What Went Wrong?

http://www.talkcomposites.com/Topic12513.aspx

By whitecel - 8/10/2014 4:13:28 PM

Hey guys,
  I decided to make the other side of my fork guard for my motorcycle today and the infusion looks to be a disaster.  Did a 30 min drop test and it was fine.  For some reason my dumbass thought that with the MTI hose you didn't need to degas the epoxy so I figured I shall try without degassing.  I always degassed even with the MTI hose.  So after I infused the part, about 30 min later, the bubbles seemed to be back flowing in the peel ply.  Is this due to not degassing and the bubbles expanded when the epoxy was setting?

2 layers of 5.7 oz cf twill
2 layers 7.5 oz Matt fiberglass
Peel ply
Green mesh
MTI hose




By andygtt - 8/22/2014 1:26:46 PM

To me it looks like you had a bridge in that area on laying the material... my experience is these sized bridges never fill with resin and whilst the material will wet out as yours has done (so structural integrity is still present, the finish and shape is compromised.