Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Mould Making
Plan to make 2 piece mould for spoiler, your comments please!
http://www.talkcomposites.com/Topic12386.aspx
By Bonobo
-
7/25/2014 11:21:39 AM
Here is the design
Here is the plug still in progress
here is how I intend to make the moulds and produce the part
By FLD
-
7/25/2014 11:25:53 AM
Looks like a perfect plan to make a perfect part. Gets my vote.