Talk Composites - The Forum for Advanced Composites

How do i make the inside of the part ?

http://www.talkcomposites.com/Topic1192.aspx

By rowaner2002 - 4/2/2012 12:09:59 PM

Hi 
Im looking to find out about making the inside of a piece,
like i can make the out side of the part to be molded in carbon etc, but its theinsde that has me abit confused .
As in the part needs to be have screw holes on the inside of the carbon mold , 
ive found this picture on the net, (dont mind the hole in it someone else owns this picture.

its the plastic screw holes that allows you to screw the panel to each other that im finding hard to do
Any ideas ?

Thanks

htthttp://img18.imageshack.us/img18/170/screwholess14armrest.jpgp://http://img18.imageshack.us/img18/170/screwholess14armrest.jpg