By wozza - 6/9/2014 8:58:01 AM
Much of my daily work is rapid prototyping/proof of concept projects. This is a small air intake. The two small dimples either side of the inlet meant a split mould and a separate mould for the underside of the part. Getting two layers of 450 plus peel ply and mesh in the deep recess without bridging was a challenge. The pressure was on with this one, two days from start to finish. 
Warren
|
By Hanaldo - 6/9/2014 5:19:34 PM
Nice work Warren. This is quite similar to something I am working on at the moment. Will post pictures when it's finished.
|
|