By ULB_qd - 6/4/2014 2:22:03 PM
Hi all,
I haven't find a topic about silicon kit, so I am posting here.
I have a problem with my silicon molds. I will try to explain the situation...
I bought on the Easycomposite website the Silicone Mould Resin Casting Starter Kit and then CS2 Condensation Cure Silicone Rubber to have more silicon for our experiment.
I create several silicon rectangles (ex: 15cmX10cmX3cm), taking care about the instructions. It is very simple and the results are what I expect and look perfect.
But...
After several days, even 2 months later, the "skin"/surface of my silicon molds are becoming "oily"... You know, when you put your finger on a surface and you can clearly see after your fingerprint on it. I can clean the surface with an alcohol solution, its works. But still after several days, all my molds are becoming "oily" again...
Is-it normal ? If yes, what kind of new and simple material can I use ?
Please help. I just need a simple silicon mold with a clean and proper surface at any time.
Regards,
Quentin
|
|